Also: liner, sleeve, Nikasil, Alusil, plasma-sprayed bore
The cylinder liner or bore coating forms the surface that pistons and rings run on. It is either an inserted sleeve, usually cast iron, or a coating applied directly to the aluminium of the block.
Wet and dry liners
Dry liners are the most common type. They are surrounded by block material and have no contact with coolant. Wet liners have coolant flowing directly around their outside. They cool better and more evenly, but make the engine less rigid. HP Academy notes that aluminium blocks usually have an iron liner in each cylinder for the rings to run on.
Coated bores: Nikasil, Alusil, plasma
Nikasil is an electroplated nickel layer with embedded silicon carbide particles, introduced by Mahle in 1967. Alusil, by contrast, is a hypereutectic aluminium-silicon alloy with about 17 per cent silicon. No layer is applied here: aluminium is removed from the surface so that hard silicon particles are exposed for the rings to run on. Pistons for Alusil bores usually have an iron-based coating on the skirt. Alusil engines include the Porsche 924S, 944 and 968 and the Mercedes M119.
With a plasma coating, a running layer is thermally sprayed onto the bore. TWI gives a layer thickness of 140 to 200 µm and explains that liners can be dropped and the walls between the cylinders made thinner. The Nissan VR38DETT has a 0.15 mm plasma-sprayed bore. Oerlikon Metco lists production use in the VW EA211 evo, the Audi TT RS five-cylinder and a Porsche V8 turbo.
In practice: rebuilds and power upgrades
The bore surface decides which parts fit. Nikasil bores need compatible rings, because the chrome rings common with cast-iron bores are not suitable. Damaged plating has to be stripped before the bore can be machined and replated. An iron liner, on the other hand, can be bored oversize, or the cylinder can be bored out and fitted with a new sleeve.
Before pistons, rings or an oversize are chosen, it should therefore be clear what bore surface the engine has and what machining the engine builder offers for it.
Common problems
- Nikasil: attack by high-sulphur fuel, as on early BMW M52 engines.
- Alusil: scoring when the exposed silicon particles break down, with higher oil consumption and piston noise.
- Pistons or rings fitted without approval for the existing bore surface.
Related terms
- Cylinder block
- Overboring and increasing displacement
- Piston
- Piston rings and end gap
- Open deck, closed deck, semi-closed deck
Related engines
Block & bottom end fundamentals → Glossary A–Z →
Sources (9)
- https://en.wikipedia.org/wiki/Cylinder_liner
- https://en.wikipedia.org/wiki/Engine_block
- https://en.wikipedia.org/wiki/Nikasil
- https://en.wikipedia.org/wiki/Alusil
- https://www.twi-global.com/media-and-events/insights/plasma-coating-of-engine-block-cylinder-bores
- https://www.oerlikon.com/metco/en/markets/automotive/cylinders-and-piston-rings/
- https://en.wikipedia.org/wiki/Nissan_VR_engine
- https://en.wikipedia.org/wiki/BMW_M52
- https://www.hpacademy.com/courses/engine-building-fundamentals/engine-anatomy-engine-block/
Want this on your car?
Calibration remotely via datalogs or on the dyno, with Link, Haltech, MaxxECU, Ecumaster or EcuTek. Send me vehicle, ECU and goal.
Last updated: